Ishack
Mechanical
- May 8, 2013
- 48
Is it permitted to use of UNS S20910 hot rolled material for stem as per NACE MR 0175 Part 3 without any hardness requirement as per table A.3. I understand from the table A.3 that the S20910 can be used without hardness requirement. Hardness of Max 35 HRC is only applicable when the above material is cold worked preceded by solution annealing. Pls clarify