I want to know why we use both of Permanent Reference Electrode and Portable Reference Electrode in Impressed Current Cathodic Protection? Why don't we use the Portable lonely? Indeed Why do we use the Permanent one?
Thanks.
 
Replies continue below

Recommended for you

Typically we use permanent only to monitor problem areas (such as suspected interference locations) or perhaps a critical location, generally where we need to take readings more often. So you could install a permanent electrode and take readings and have someone monitor it at a specified fequency, even hook up a datalogger, the CP vendor can use this data in analysis, or have compamnies own people monitor rather than calling the CP vendor every time. As far as the readings between permanent and portable, they are the same (assuming electrode type is the same).
 
Thank you very much brimmer. It was helpful.
 
Over the years , it has been observed that the permanent reference electrode those not really last more than two years
 