I need to bond molten lead to the inner diameter of cast iron housing. The molten lead will be poured in the housing and it will acts as a gas seal. Will it seal or do I need some platings or coatings? The operating temperature is around 400 degree F.
 
Replies continue below

Recommended for you

Lead has been used in the plumbing field to seal cast iron drainage pipes.

So there will be a seal, but whether it will be gas tight, I am not sure.
 
Do not forget the PPE in this task. The fumes form liquid lead will exceed the PEL.
 