Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

[Urgent] Subroutine which changes the Young's modulus according to changes in Engineering Strain

Status
Not open for further replies.

kooshaa

Mechanical
Joined
Mar 25, 2016
Messages
15
Location
DE
Hi Everyone.

The model that I am currently trying to simulate in abaqus has a material that its Young's modulus (E) is decreasing with the increasing of the engineering (total) strain. I tried to write a VUSDFLD subroutine (my model is Dynamic Explicit and since I am an absolute beginner with coding I would like to avoid VUMAT).
I found an old thread here ( which gave me some clue in what I should write (Although they used USDFLD subroutine).

Here is my VUSDFLD subroutine:

Here are my questions:
1- The young's modulus of my material model in changing with the engineering strain (which contain both elastic and plastic strain). Does my subroutine cover both parts? and did I use right codes for it?

2- Should I just add the Data written below in the Elastic section of material property module (since it also contain the plastic strain)? and if I do so, would abaqus recognize when the strain reached the plastic zone?

E ------ Engineering Strain
203050 0
186750 0.01
174750 0.02
168450 0.03
163900 0.04
159800 0.05
156100 0.06
152850 0.07
148950 0.08


(I made this new thread due to the wrong topic that I chose for the previous one.)
 
and is there any need to convert my experimental data to true strain?
 