Hi,
I need some help to source a pipe fitting for my power station. If someone has one or can give me details of good reputable suppliers please. We would be willing to buy or replace it as soon as my usual supplier delivers to us (he is currently quoting 4 weeks!). The fitting needed is:-

Fitting Type – Eccentric reducer
Material – P91 (X10CrMoVNb910 / 1.4903)
Nominal Size – 65mm to 50mm
Physical size (OD x Thickness) – 76.1 x 10.0mm – 60.3 x 8.0mm

If an eccentric reducer is not available then a concentric reducer could also be used.

The application is for a high temperature steam pipe. The old reducer has failed due to problem with a valve.