Hi can anyone help me out on how a uPVC pipe will be connected to HDPE pipe. Im currently designing an irrigation system wherein the client requires us to use uPVC pipe for sizes below 225mm and HDPE for above sizes. Much will be of help if you can give me commercial sizes and specs of uPVC in spreadsheets. Thanks
 
What size is your HDPE pipe. You could butt-fuse a reducer and flange adapter and backing ring onto the HDPE pipe and have a simple flanged connection. There are lots of vendors for those fittings.
 
Hi thanks guys for the info. Yap its a pressure system the HDPE DN 315mm will be connected to uPVC DN 125mm and DN 100mm pipe
 