I need to know the following regarding WCB and LCC Steel (Valve Body).
1. Is WCB acceptable for NACE?
2. When Stress relieving WCB material, does the final product have the same properties as LCC material, and does it conform to NACE stds?
2a. What is the upper most temperature limit for the material if it does conform to nace specs without compromising the structural integrity?
3. At prolonged use above 600°F, Do the characteristics of HT TRT WCB material start to degrade? And does it start to form graphite at 700-775°F?
4. When using WCB that has been heat treated, and when using at the upper temperature limits (650°F) for long periods of time what effect does this have on the structural integrity of the valve body (valve body is heat treated WCB)?
1. Is WCB acceptable for NACE?
2. When Stress relieving WCB material, does the final product have the same properties as LCC material, and does it conform to NACE stds?
2a. What is the upper most temperature limit for the material if it does conform to nace specs without compromising the structural integrity?
3. At prolonged use above 600°F, Do the characteristics of HT TRT WCB material start to degrade? And does it start to form graphite at 700-775°F?
4. When using WCB that has been heat treated, and when using at the upper temperature limits (650°F) for long periods of time what effect does this have on the structural integrity of the valve body (valve body is heat treated WCB)?