Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Updating a very, very old Negri Bossi

Status
Not open for further replies.

AG8

Mechanical
Joined
Jul 19, 2009
Messages
1
Location
CA
We are installing a microprocessor based controller on an old "Piston - non screw" Negri Bossi R5 machine.
Has anyone "out there" have any experience with this machine ?
What purpose does retracting the barrel from mold contact between cycles , have ? Better Cooling ?
 
Well, the barrel is heated, and the mold is cooled, so it makes some sense to not have the machinery fighting itself when it doesn't have to.
... on the other hand, retracting the barrel on every cycle introduces some complexity.

Since you're adding fancy controls, you could presumably program the machine to work either way, and see how it works out for you.



Mike Halloran
Pembroke Pines, FL, USA
 
Retracting the barrel during (usually, but not exclusively) cooling is called "sprue break".

Often used to keep nozzle tip hot to stop it freezing off and preventing injection on next cycle. Also used with some materials to stop "stringing" of the sprue when tool opens, causing the runner system to hang in the tool.

I would suggest it's important.

H

www.tynevalleyplastics.co.uk

It's ok to soar like an eagle, but weasels don't get sucked into jet engines.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top