Here's the story. This parts are made using 17-7ph sheet stock (AMS5528 or MIL-S-25043) which is cut into strips and then heat treated to TH1050 IAW Mil-H-6875. The parts are then formed using fine blanking process. The failure occured while theres parts are in opperation. They link together with one another and form a chain. We know that maximum normal opperating loads are 300 lbs and testing has shown these links failure at a minimum of 750lbs. This loading can't happen in reality because there is a weaker part which would fail first. These "links" were brand new so I can't imagine fatigue is the issue. Hardness was slightly high on the links @ Rockwell C 47. AMS 2759/3D says piece parts should be 38-44 HRC which covers heat treat of parts. AMS 5528 covers the raw material and its "responce to heat treatment" They indicate a range of 38-46 HRC. The failure surface is almost parallel with the sheet plane without necking. This is different from links that we tested. Any thoughts from the experts????

 
Michael,

Would this be possible at a sheet thickness of .032"?

Thanks,

Mark Vose
 
Sure, rolling only thins layers proportionately. This happens often with martensitic stainless, such as 420,for thin blades, like scalpels. 17-7 is quite similar. The layer may seem thin on a macro scale, but to get rid of the centerline layer by evening out the composition through substitutional diffusion is a tall task. It helps to have a continuous caster with electro-magnetic stirring or to cast with low superheat. You should make the absence of continuous centerline ferrite part of your spec.
Ferrite is the Achilles heel of PH grades. 15-5, 13-8, and Custom 450 are better in this regard.

Michael McGuire
 
Michael,

Thank you for the information. I think we're on to something. I'll post something when I get lab results. We get to see if our suspitions are correct!!!

Thanks again,

Mark Vose
 
Mighoser -- See this thread also:

thread330-96298

Nick
I love materials science!
 
NickE,

Did you find the source who provided the bad material? I wonder if my 17-7 was produced by the same company?

Mark
 
Nope, didn't even look. One of our prototype vendors caught the problem. We sent the parts (except inspection samples)back and the vendor re-made them using a different heat of material. (at least)....

Since we were not buying this directly from a mill or even a secondary house there was no need to pull out the implements on the source...

I'd bet that 17-7 stays on the market a decent amount of time, could be very likely that the heat that made my .050" could have made your .032"

Nick