Proximity of exhaust pipes and catalytic converter can have a profound effect.
Apart from being close to the exhaust, many areas allow the use of filled polypropylene components which would imply a bit over 100 deg C. some areas need nylon which implies long term temperatures between 100 and 130 deg C with short term spikes not going over about 150 to 160 deg C
Nylon fails close to the exhaust which implies 160 to 200 deg C for a moderate amount of time (maybe 100 hours exposure)
Regards
pat pprimmer@acay.com.au