Hi all,

I would like to hear any opinion in the subject of Ultrasonic inspection in composite laminates having a metallic insert or shim.

I have heard about some Ultrasonic inspections where the shim is not detected, some of the theories is that the composite/metal compaction is good that the ultrasonic inspection is not able to capture it.

Thanks,
 
Replies continue below

Recommended for you

albertoruenes...

There is an important aspect to composite solid laminate or sandwich structure Inspection [especially US-NDI] for critical parts/structure: NDI reference standards must be developed and used during the process, to minimize potential for 'missing an element or defect'. These standard must have built-in defects, and/or 'features', so that the NDI tech can refer-back-to-them for comparison/reference.

See SAE ARP5605 Solid Composite Laminate NDI Reference Standards

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 