Does anyone know if this grade is included in the latest revision (2005) of this standard? I only have the 2002 revision and it does not appear in this one. This seems a little odd since the 1998 version of JIS G 4303 includes it. Any background would be appreciated.
 
TVP--No 303Cu grade listed. Only copper containing grade is UNS20300 (XM-1)with 1.75-2.25 Cu. Of further interest--After the A 582/A 582M-95b title block it reads further "(Reapproved 2000)" But then there is a footnote, stating that Table X1.1 was editorially corrected in May of 2003.In looking at Table X1.1, there is no clue as to what the correction was.This is all straight from the 2005 edition of Volume 01.03
 
Thanks Steve. I appreicate your assistance.
 