Good day Eng-Tippers

I searched the forums, but could not find a relevant thread.

What are your experiences with the use of tubing vs hard piping for instrument connections in very high pressure applications (Cl 1500 & Cl 1500)?

We're currently considering both options, and would like to get an idea of 'industry standard'.

Regards,

maraisjo
 
Class 1500 isn't actually all that high pressure for stainless steel tubing. It is well within the limits of ordinary 2-ferrule compression fittings. Hard pipe is a disaster for instrument impulse lines because it is so inflexible to change. Some end user clients use it on large lines and vessels. I can see the benefit for root line sizes say 12" and larger, and vessels greater than say 8' in diameter, but the benefit for line sizes and vessels smaller than that is specious at best in my opinion.

"High pressure" to us is beyond 2500# class. Then you're into either pipe with Grayloc type closures, or tubing with cone and thread closures. Such "tubing" is basically pipe, just with a different method of end connection, and it typically has a wall thickness which approaches its ID.
 