I am running with an issue for tube-tubesheet joint. It is a double tubesheet heat exchanger. Tubesheet hole is provided with two grooves for tube expansion.
Hole diameter = 0.756"
Tube OD = 0.75"
Tube Wall Thickness= 0.049" ( Avg).
Tube material= Seamless titanium SB 338 Gr 2
Tubesheet material = SA 240 GR 316 L
Expansion is performed in back tubesheet but still it is leaking. Is there a way to make it leak proof?
Please advise
I am running with an issue for tube-tubesheet joint. It is a double tubesheet heat exchanger. Tubesheet hole is provided with two grooves for tube expansion.
Hole diameter = 0.756"
Tube OD = 0.75"
Tube Wall Thickness= 0.049" ( Avg).
Tube material= Seamless titanium SB 338 Gr 2
Tubesheet material = SA 240 GR 316 L
Expansion is performed in back tubesheet but still it is leaking. Is there a way to make it leak proof?