In order to do plasticity analysis on metals, you need to put in the correct data in abaqus. So far, I have an example from Simuleon website and Dowling (Mechanical behaviour of materials, 4th edition). I find the very high values very strange, can someone explain? See attached file...

I am unsure of the yield point, as I think this should be at 0,02% offset, but that is from the calculated E module, right?
 
 https://files.engineering.com/getfile.aspx?folder=a2847a08-f4b0-44d8-91b5-f60a859f9be6&file=Conversion_Engineering_Stress-Strain_to_True_Stress-Strain.xlsx
i think you used percentages for your strain values.

if you divide your strain values by 100 things should make more sense.
 
there's also quite detailed explanation of how to do this in the "Getting Started with Abaqus Guides"

Section 10.2 in both the Interactive and Keyword Editions - Plasticity in Ductile Materials


 
Dave442: Thanks, that solved it, of coourse...
 