I am experiencing an adhesive failure using a silver filled epoxy. The bond has an adhesive failure at the nickel plated surface. The aluminum part is plated with a med phosphourous nickel. The same epoxy bonded to stainless steel has twice the bond strength and cohesive failure. any suggestions?
 
Replies continue below

Recommended for you

In hybrid chip & wire assembly we used a plasma cleaner immediately prior to die bond with a silver-loaded epoxy. Substrate was either Pd-Ag, gold, or a low-temperature glass, and the plasma cleaning was to remove any organics on the surface which could weaken the bond.


----------------------------------
image.php

If we learn from our mistakes I'm getting a great education!
 
Surface contamination is the root of most bonding problems as you probably know. I would get a SEM and a scan for surface elements. I would also try Boron Nickel. That sometimes bonds better.
 