My clients requirement is 10" swing check valve with A216 WCB body & Trim 1. I supplied valve with A216 WCB + 13% Cr for the trim. My client has rejected informing that he asked for trim 1 but I have supplied trim with A216 WCB + 13% Cr. Can any of you give me an idea how I can convince my client to make him accept the supplied valve
 
Replies continue below

Recommended for you

Ask your customer about the medium, pressure and temperature for the application, and then decide whether trim 13%Cr is adequate. You cannot generally say that one trim is better than another, as each trim has been defined for a certain set of applications and conditions.

My focus: Alloy Valves Super Duplex Valves Monel Valves Incoloy Valves [link titanium-valves.com]Titanium Valves[/url] Hastelloy Valves
 
If (1) the customer required you to supply a valve with Trim 1, (2) you accepted their order without specifying that you would supply trim 13%Cr, and (3) you actually supplied something different then contractually agreed, it is within the customer's perogative to reject what you supplied and to hold you liable to supply what was specified in the contract.



Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
"Trim 13%Cr" doesn't really tell the customer anything it is too generic. you need to define the material of the disc facing , seat ring facing, and the hinge pin.

Trim 1 is 13%Cr seat and disc. You have to demonstrate that there is a 50Hb differential between the seating surfaces and that the nominal hardness is 250.

So if your disc is 250 HB the seat ring must be 300HB or more.

Once you prove this it's possible your customer may accept the valve.
 