I require gate valve WCB body with trim 2. I am getting offer with the below specs:

wedge: WCB+304
Stem: F304
Seat: A105+304

When I had a look in to API 600 for trim 2, it mentions the below for seat:
A 351 (CF8) in cast form or A182 (F304) in forged form. I am confused why the manufacturer is offering A105+304 for seat. He is saying he has offered as per trim 2, but I do not understand how & he does not give a proper reason. Can any one help me.
 

Ask the supplier both for reasons and drawings with details.

 
API 600, API 603, and API 602 also allow weld deposited 304 on the seats to meet trim 2 requirements which is what it appears your drawing is implying.

 