Hello,
We have tried injecting small dosages of Chlorine into a Treated Water Tank at an NGL Plant, in addition to the injection of the Biocide. The results were marvelous and the bacteria was dramatically decreased.
However, I wonder if there is cons and pros for continuing injecting the Chlorine inside the Tank for the process and the equipment, factoring that the treated water is used as a cooling medium in a closed circuit.
Thanks and best regards
We have tried injecting small dosages of Chlorine into a Treated Water Tank at an NGL Plant, in addition to the injection of the Biocide. The results were marvelous and the bacteria was dramatically decreased.
However, I wonder if there is cons and pros for continuing injecting the Chlorine inside the Tank for the process and the equipment, factoring that the treated water is used as a cooling medium in a closed circuit.