I am on a mission to find a replacement injection moulding polymer to replace the current Cycoloy (PC +ABS) blend.
We have parts that are failing due to an impact force and we have changed the geometry as much as it allows to get rid of stress concentrators and to better distribute the forces, however we would like to see if we can also improve the properties by using a different material.
Does anyone know of a polymer which would have similar Flexural modulus to Cycoloy (2.6GPa) (between 2 and 3Gpa), Flexural Yield strength of more than 80Mpa and greater toughness than Cycoloy. Izod Notched (ASTM D 256) for Cycoloy is 5.3J/cm or 10ft-lb/in.
I have found some Polycarbonate/PET and Polycarbonate/Acrylic blends which look like they would do the job, but I wanted to see if someone could recommend something else?
Thanks in advance!
We have parts that are failing due to an impact force and we have changed the geometry as much as it allows to get rid of stress concentrators and to better distribute the forces, however we would like to see if we can also improve the properties by using a different material.
Does anyone know of a polymer which would have similar Flexural modulus to Cycoloy (2.6GPa) (between 2 and 3Gpa), Flexural Yield strength of more than 80Mpa and greater toughness than Cycoloy. Izod Notched (ASTM D 256) for Cycoloy is 5.3J/cm or 10ft-lb/in.
I have found some Polycarbonate/PET and Polycarbonate/Acrylic blends which look like they would do the job, but I wanted to see if someone could recommend something else?
Thanks in advance!