one of sales people came in with a request on a casting using "TOMISILL white Brass
?? can any one help me in ID-ing this metal?? all help much appreciative
 
Replies continue below

Recommended for you

Tomisil
White Brass
UNS C99700

C 56.5%
Mn 12%
Al 1%
Ni 5%
Pb 1.5%
Zn 24%
 
i thank you
we found out the sales guys spelled it wrong
it is \tombasil white brass, leaded, is there a lead free = to this??
 