Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Titanium-Zirconium welding

Status
Not open for further replies.

khalidkhattak

Mechanical
Aug 27, 2002
22
Some body there tell me about welding of zirconium to titanium. Any related website for information.
 
Replies continue below

Recommended for you

The following information is reported from ASM Handbook Vol. 6:

ZIRCONIUM is a corrosion-resistant structural metal that has many physical and mechanical properties similar to titanium. The metals and alloys based on zirconium and tantalum have weldability characteristics similar to those of titanium. Zirconium can only be welded to itself or to other reactive metal alloys, such as titanium, niobium, or tantalum.

 
Both Ti and Zr can be welded to one another. Both alloys require extreme cleanliness and protection from contact with the atmosphere during welding. Here is some information to review;









I would consider an SFA 5.16 ERTi-2 filler metal with the GTAW process. The root and weld must be shielded at temperatures above 500 deg F during welding. In some welding applications, a gas tight chamber is used to assure prevention of contamination from oxygen, nitrogen or hydrogen gases for Ti and Zr.
 
Do a web search on Teledyne/Wah Chang, they are a major manufacturer of zirconium.
 