Dec 13, 2007 #1 bmoorthy Mechanical Joined May 29, 2003 Messages 457 Location CA B 16.5 does not address Titanium flange. Suppose one needs 150 Rating 6" Titanium Flange, where can one find the pre published allowable stress at 100 Dec C?
B 16.5 does not address Titanium flange. Suppose one needs 150 Rating 6" Titanium Flange, where can one find the pre published allowable stress at 100 Dec C?
Dec 14, 2007 #2 TGS4 Mechanical Joined Nov 8, 2004 Messages 3,986 Location CA As recommended by Annex B of the 2003 Edition, you should check with ASME Section II, Part D. Upvote 0 Downvote
Dec 14, 2007 #3 TGS4 Mechanical Joined Nov 8, 2004 Messages 3,986 Location CA Oh - and the Standard is an ASME standard so the appropriate designation for the Standard is ASME B16.5. (Not ANSI)... Upvote 0 Downvote
Oh - and the Standard is an ASME standard so the appropriate designation for the Standard is ASME B16.5. (Not ANSI)...