hi gsberger,
The volume of a tire depends on the construction and the size.For truck tire of size 10.00 - 20,that is section width of tire is 10 inches and curing ring dia is 20 inches,the volume is around 30000 cc.if u consider the specific gravity to be 1.2 then the weight would be 36 kg
Jeyakumar
R & D
Ceat Ltd