Dear Sirs,

One of my customer want to buy motorcycle valve made by Ti 6242, my problem is this material can not be found in Asian area.

Is anyone can tell me where can by this material and the benefit of using Ti6242.

Thank you in advance.



 
Supposedly the better Ti engine valves are made in Russia. Do a search on this site as they have been mentioned in one of the Automotive Forums.
 
Try Nippon Steel. The following links are to a technical article on Ti alloys for auto apps (including Ti6242 for exhaust valves) and to the contact page for NSC locations not in Japan. Click on "Head office" at the top of the page if you want to contact NSC in Japan.



Other producers of Ti6242 are Deutsche Titan and TIMET. TIMET is the leading producer. The following links have more information:


 