Good morning, we are designing a pressure vessel and at one point we have three weld seams that coincide. Does anyone know if there are limitations in the codes (no matter ASME or EN) to this?

Regards,
 
Replies continue below

Recommended for you

We've built many spherical heads for ASME pressure vessels where 3 welds come together in a Y shape.

If that's not the configuration you're talking about, perhaps a sketch would help.
 
You would rather avoid that situation if possible, not least from the constructability and inspectability perspectives.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
See Sec VIII, Div 1, UW-9(d), if applicable, for long seam separation.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
MGZmechanical.
If this happens to you in design it means that you are working poorly. Change the design instead of looking for help elsewhere.
 
Thank you for you help. It is something like the picture attached but the horizontal flage goes to the outside of the vertical flange. So we have the longitudinal seam, the circumferencial and the one to weld the vertical flange to the horizontal one.

Regards,
 
 https://files.engineering.com/getfile.aspx?folder=ecbe2853-82da-4f88-90d9-8d91f90af65a&file=1.png