Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

three pieces of sheet welded together to make a dish end , is it right ? help me

Status
Not open for further replies.

AhmedDeiaa

Mechanical
Joined
Nov 1, 2014
Messages
29
Location
EG
please can any one tell me , what is the recommended welding procedures for forming a dish end (Head)consist of three pieces of sheet welded together with final outer diameter = 3100 mm
it would be preferred if there is a standard for this .
 
There are numerous standards for welding, there is not "a standard" to weld all materials in all thicknesses by all methods using all equipment.

First step, confirm if there is any quality control program or process at the facility. If so, review it.
Secondly, confirm what codes or standards are applicable to the finished product. Review those standards for any limitations on welding procedures, etc. The standards may limit the number of pieces that can be used.
Thirdly, confirm if your company has ever qualified weld procedures or welders per the standard in question. If so, your best options are to use procedures already qualified and welders already qualified.
If necessary, you can check with your welders and see what methods, thicknesses, materials, etc., they are comfortable using, set up welding tests to qualify the corresponding procedures and take it from there. The correct welding is that which can be done quickest, most economically, and fulfill all quality requirements, and may vary depending on the personnel and equipment available, as well as on the material and codes being used.
You also want to looking into weld examination (radiograph), and any forming issues (annealing or stress relief, etc.).
I think a lot of heads in that size range are seamless; I was thinking most non-seamless heads were made in just two pieces, but I'm not sure what the options are.
There are certain pre-qualified procedures available in some cases, also.
The question is very very vague, and more specific information may get you more useful answers.

 
Check the UW-12 for using a butt joint with full radiographic exam, which to have the joint efficiency = 1.0.
 
Come on. What pressure, what temperature process fluid, what metal? What specification are you working towards? What are you going to do with the assembled part?
It is a bit absurd to think we can legitimately and accurately recommend a weld process for three pieces of unknown metal for an unknown application to serve under unknown conditions.
 
JStephen (Mechanical)
the second thread is completely different compared with the first one ,

the first one was about welding process in dish end

the second one is about crowing the dish end not welding ...........thanks JStephen (Mechanical)
 