Oct 11, 2010 #1 mielke Mechanical Joined Aug 24, 2009 Messages 181 Location US any suggestions on drill hole size for a 1/2-13 thread mill. It'll be in 3/4" thick 304SS. We had some problems in the past with this material using a cut tread and had to open the hole larger than recomended.
any suggestions on drill hole size for a 1/2-13 thread mill. It'll be in 3/4" thick 304SS. We had some problems in the past with this material using a cut tread and had to open the hole larger than recomended.
Oct 11, 2010 Thread starter #2 mielke Mechanical Joined Aug 24, 2009 Messages 181 Location US from what i've seen you drill the the minor diameter size. anyone have any experience with this? Upvote 0 Downvote
Oct 11, 2010 #3 mcgyvr Mechanical Joined Aug 8, 2006 Messages 1,457 Location US http://www.shender4.com/thread_chart.htm Upvote 0 Downvote
Oct 11, 2010 #4 mrainey Industrial Joined Jun 22, 2002 Messages 225 Location US The thread mill doesn't cut the minor. You machine it first to be within the size limits required by the standard. Software For Metalworking http://closetolerancesoftware.com Upvote 0 Downvote
The thread mill doesn't cut the minor. You machine it first to be within the size limits required by the standard. Software For Metalworking http://closetolerancesoftware.com