I have 2 old jugs of LPS3 that are much thicker than I recall. I'd like to thin the LPS3 with some solvent that will evaporate harmlessly (to the LPS3) after application.

Suggestions?

thanks

Dan T
 
It's "thickish" anyway. I'm not sure about solvents. Can you pull up an MSDS sheet? Take small batches and try different solvents? Perhaps try LPS1 as a solvent?

Rod
 
Component
CASRN
Weight Percent

Aliphatic Hydrocarbon
64742-47-8
60 - 70%

Distillates Petroleum Hydrotreated Heavy Paraffinic
64742-54-7
5 - 10%

Propylene Glycol Mono-n-butyl Ether
5131-66-8
5 - 10%

Dipropylene Glycol Mono Butyl Ether
29911-28-2
1 - 5%

Light Mineral Spirits
64742-88-7/8052-41-3
1 - 5%

You could add a little more mineral spirits
 