Hello everybody,
We are currently using for our injected products a thermoplastic produced by Bayer, BKV 50 H2.0 . We have tested some other plastics in order to get a more shiny finishing of parts surface as injected but could not find an acceptable one. And it is not because of mold finishing !
As long we are not going to change the technology could somebody guide me to a suitable material that will keep closed the mechanical and pysical properties but will give me a shiny finish ?
Thanks in advance!
We are currently using for our injected products a thermoplastic produced by Bayer, BKV 50 H2.0 . We have tested some other plastics in order to get a more shiny finishing of parts surface as injected but could not find an acceptable one. And it is not because of mold finishing !
As long we are not going to change the technology could somebody guide me to a suitable material that will keep closed the mechanical and pysical properties but will give me a shiny finish ?
Thanks in advance!