When is required that all plates shall be supplied using the thermo-mechanical control process (TMCP), automatically the supply status of the material will be the type thermomechanically?
If it instead the plates to be transformed into pipes, instead talking about Thermomechanically rolled? Is it correct?

Thank you in advance,
Emilio
 
By the appropriate material specification that is referenced.
 