Hi,

I am trying to find a supplier of thermally conductive EVA.
I would like to try laminating solar cells with it.
Does anyone know a vendor ?

Thanks, Thierry
 
Replies continue below

Recommended for you

You need to keep it transparent I assume? If so that's a much harder challenge. If not then contact Jon Leist at Momentive who make hexagonal boron nitride, a filler used to increase thermal conductivity.

Chris DeArmitt PhD FRSC CChem

Consultant to the plastics industry
 
Hi Chris,

thank you for your input. I do not need it to be transparent so it might work.

Best,
Thierry
 