Does someone know a coating that could be applied on cooling elements resistent againts seawarter and in such a way that it maintain thermal heat transfer.
 
Replies continue below

Recommended for you

hebco

What you want to do is a apply a coating that is salt water resistant and has a high conductivity. If you do a "Google" search, using the bolded words, you will find companies that sell such products.

Patricia Lougheed

Please see FAQ731-376 for tips on how to make the best use of the Eng-Tips Forums.
 
I think it has to be resistant to bio-fouling, too.