The manufacterer of the stripper overhead accumulator has choosen the material of shell and head astm a- 387 gr22 cladding with monel although a-387 is good at elevated pressure and temperature . I don't know what the reason of using cladding for monel.
 
Monel would prevent corrosion due to condensation, which is basically acidic corrosion.

DHURJATI SEN
Kolkata, India


 
Cladding is a way to get the high corrosion resistance at a lower cost

--- Best regards, Morten Andersen
 
You are welcome,..... ENGRANIA

MJCronin
Sr. Process Engineer
 
@ENGRANIA
"stripper overhead accumulator" - what does this stripper strip and what does this accumulator accumulate?
 
Engrantia

Monel cladding is for corrosion purposes, but in what service will be aplicated the stripper overhead vessel?