In a single lap shear test specimen, does altering the gauge length (or the overall length of the specimen) have any effect on the peel stress? ie) would a longer specimen produce a greater peel stress, and cause the specimen to fail sooner?

Thanks.

 
Replies continue below

Recommended for you

Is the specimen thick enough to load the adhesive/weld/whatever in pure shear, without bending?
 
No, a slight amount of bending occurs.
 
Sorry, I forgot to mention. Assuming the bond area remains the same, just altering the gauge length of the specimen. I know that altering the bond area effects the level of peel stress, but does altering the gauge length effect it?

Thanks for your help.
 