Good morning sir,
I need to ask you a question regarding the test of bronze bolted bonnet valves above 3 inches.(Flanged ANSI 150/ANSI 300 and S.200/s.300 npt)
For valves up to DN80 i would obviously use (for test pressures) the msssp80 standard which, as per the standard, only concerns valves up to dn80.
For valves from dn80 upwards which standard should I refer to?

I have searched for hours and hours on internet and in the standards in my hands but I have not found direct references that would make me understand which standard I could use for pressure test.
I thank you in advance.

Best regards
 
Replies continue below

Recommended for you

Well what standard or specification are you making them to??

What is their design pressure?
Usually shell pressure test is 1.5 x design pressure.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Since you mention Class 150, 300, maybe the valve standard that you could reference for testing is ASME B16.24?
 