Could anyone please explain the acceptance criteria for tension test of PTC? (interpretation of Fracture on Weld and base metal)
Design Code : ASME SEC. VIII Div. 2
Product: Column
Material : SA537 CL2
 
Replies continue below

Recommended for you

Same as WELDING PROCEDURE QUALIFICATIONS.