Hi,
I have to perform a simulation of tensile testing of PTFE(teflon). I've been given the data about the experiment (I have the stress-strain curve, Poisson's ratio, sample dimensions, strain rate). The problem is that this material is very ductile and the percent strain is equal to 246%. I work in Ansys apdl and I've been struggling with choosing the correct material model. Because I have the stress-strain curve I tried with
nonlinear -> inelastic -> rate-independent -> isotropic hardening plasticity -> Mises Plasticity -> multilinear
I just copied the points from the plot I was given (experiment data) and created the same stress-strain curve in Ansys. I know that behavior of PTFE depends on strain rate but in this case the strain rate is 0.5mm/min so I think it can be neglected at first. Anyway every time I start simulation I receive information "one or more elements have become highly distorted..." after some time. My guess is that this happens because the stress value exceeds the value from the curve (but it doesn't happen when I input true stress-strain curve). But I don't know why because the stress-strain curve becomes almost horizontal at some point (if the curve is engineering curve). My second guess is that elements' elongation is to high but have no idea how to prevent that.
Can anybody help me to solve this problem? Why I keep getting this error and what material model would be correct for Teflon in Ansys apdl? I enclosed a picture of the shape of the elements at the error step
PS I really read a lot about nonlinear simulation in Ansys, I tried so many different solution settings and it didn't help at all so the cause of the problem must be somewhere else
I have to perform a simulation of tensile testing of PTFE(teflon). I've been given the data about the experiment (I have the stress-strain curve, Poisson's ratio, sample dimensions, strain rate). The problem is that this material is very ductile and the percent strain is equal to 246%. I work in Ansys apdl and I've been struggling with choosing the correct material model. Because I have the stress-strain curve I tried with
nonlinear -> inelastic -> rate-independent -> isotropic hardening plasticity -> Mises Plasticity -> multilinear
I just copied the points from the plot I was given (experiment data) and created the same stress-strain curve in Ansys. I know that behavior of PTFE depends on strain rate but in this case the strain rate is 0.5mm/min so I think it can be neglected at first. Anyway every time I start simulation I receive information "one or more elements have become highly distorted..." after some time. My guess is that this happens because the stress value exceeds the value from the curve (but it doesn't happen when I input true stress-strain curve). But I don't know why because the stress-strain curve becomes almost horizontal at some point (if the curve is engineering curve). My second guess is that elements' elongation is to high but have no idea how to prevent that.
Can anybody help me to solve this problem? Why I keep getting this error and what material model would be correct for Teflon in Ansys apdl? I enclosed a picture of the shape of the elements at the error step
PS I really read a lot about nonlinear simulation in Ansys, I tried so many different solution settings and it didn't help at all so the cause of the problem must be somewhere else