Feb 22, 2006 #1 MalcolmA Mechanical Joined Sep 22, 2003 Messages 40 Location US Does anyone know where I can find information on the temperature limits of metal jacketed gaskets with a soft iron jacket.
Does anyone know where I can find information on the temperature limits of metal jacketed gaskets with a soft iron jacket.
Feb 23, 2006 1 #2 Goahead Aerospace Joined Jul 13, 2003 Messages 625 Location IL A commercial supplier posts the maximum temperature for soft iron at 540 C = 1000 F see page 48 at: http://www.flexitallic.com/documents/Design_Criteria.pdf Regards, http://www.welding-advisers.com/ Upvote 0 Downvote
A commercial supplier posts the maximum temperature for soft iron at 540 C = 1000 F see page 48 at: http://www.flexitallic.com/documents/Design_Criteria.pdf Regards, http://www.welding-advisers.com/