Can anyone tell me if there are any issues in designing/fabricating pressure equipment (small vessels and piping items) using stainless steel 316 (not 316L) for the following:-

The mechanical codes are either ASME VIII div1 or ASME B16.3.

Design Temps: Two Options a)538 Deg. C. b) 590 Deg. C

Fluid passing thro' the equipment is steam only.

Thanks in advance.
 
Replies continue below

Recommended for you

green1959,

Cross posting is discouraged. This helps everyone involved come to resolution, hopefully.
 
Check into the ASME Boiler and Pressure Vessel Code, Section II Materials, Part D - Properties, current Edition. I built a table based upon the 1995 edition. My notes reflect a maximum operating temperature of 1500 degree F. However, the allowable stress value avalanges from 11000 psi at 1100 degree F to 4100 psi at 1300 degree F. 590 C is just below 1100 F. Again the current Part D may be helpful.
 