Hello, the NF F 01-281 Standards refers these technical report to surface preparation in order to fit metallic inserts, does anyone know about this? Thanks.
 
Replies continue below

Recommended for you

Any indication of the source of the standard. I tried a search and got a lot of chinese characters and a reference to a hotel, among many other documents, but nothing relating to surface preparation.

regards

blakmax
 
Thanks blakmax, I saw that in a paragraph inside de French standard NF F01-281.
Regards,
 
MJM Do you have a website for the standard? I am curious.