Hello guys,
I have a couple of questions.
1- Is that necessary to apply the backing gas for root of T joint fillet welds of stailess Steel materials?
2- Considering ASME IX, is that possible to use GTAW approved WPS qualified with backing gas for a T joint fillet weld, without backing gas? Or we have to qualify a new procedure for that application. The reason is that there is no gap between parts in the back of T joint fillet weld to apply backing gas and it can touch the root of welds.
Thanks
I have a couple of questions.
1- Is that necessary to apply the backing gas for root of T joint fillet welds of stailess Steel materials?
2- Considering ASME IX, is that possible to use GTAW approved WPS qualified with backing gas for a T joint fillet weld, without backing gas? Or we have to qualify a new procedure for that application. The reason is that there is no gap between parts in the back of T joint fillet weld to apply backing gas and it can touch the root of welds.