If I have a 2" S-160 A312-304L pipe does anyone have the actual of relative installed cost difference between a socket weld ell or a butt weld elbow

A182F316L CL 6000 90 deg elbow + 2 socket welds or
A403WP304L S-160 90 deg elbow + 2 butt welds

while I am at it, would the cost for S-80 and CL3000 fittings be much less?

thanks
Mark
 
Replies continue below

Recommended for you

That may not be the only consideration.

The engineer may want to avoid the SW elbow due to the higher SIF.

Regards, John
 
pipe..

Welders in the field do not like small, butt-welded things.

Socket (fillet) welded piping components are much easier and usually cheaper. Virtually all welders on a crew are qualified to perform socket welds, fewer are certified to perform butt welds.

When a root purge gas is involved, (like is required for SS pipe for example..) it gets more complicated.