Hi,
All long story short I have a mechanical engineering hands on background, but what will be a best source to collect and gather information on the manufacturing process for PMC-790 shore 90A?
So far I have Industrial vacuum degassing, pouring compound to a aluminum mold as an example, cure time 48hrs, post cure 4 to 8hrs at 150F.
If I missed information in between I am all ears thanks.
Juan
 
Replies continue below

Recommended for you

There's a shed-load of information on the internet if you google PMC-790.
 