We make and test replacement pumps for the petrochemical industry. As a part of the testing process, we have to hydrostatic pressure test each pump case. I am looking for wetting agent or surfactants that you add to the water when pressure testing to enhance the properties of water.

Does any have an idea where I could find this product and who manufactures it?

API 610 mentions the use of Wetting agents while pressure testing but does not tell any thing more.

I appreciate your input.

--------------------------------------
There is always some thing better out there...
Mahadhatu
 
What properties are you trying to 'enhance'?

<<A good friend will bail you out of jail, but a true friend
will be sitting beside you saying ” Damn that was fun!” - Unknown>>
 
To reduce the surface tension of the water to increase its sensitivity to cracks or other defects in the casing.

--------------------------------------
There is always some thing better out there...
Mahadhatu
 
Typically only used for pressure testing with water, when the pump actual service is high temp (500 F or above), or low SG (0.7 or less).
 
Thats right. We currently use kerosene for testing pumps at room temperature that operate over 500F or low SG.

Betz laboratories is the one in Pennsylvania ?

--------------------------------------
There is always some thing better out there...
Mahadhatu
 
you can try Kodak as well. Used in film processing - go figure
 