Dear all
We are facing a different problem in induction of rock shafts of tractor.we have inductotherm medium frequency induction hardening machine. we required 2.5 mm to 3 mm case depth at 45 hrc in there and surface hardness is 50 hrc after tempering.we are getting proper depth when u cut the section and check but surface hardness is varying alot when we check on splines.our polymer ratio is 5% to water..please advise.
regards.
 
What is your method for determining surface hardness?
 
Are you evaluating the surface of the steel shaft before hardening? Is there decarburization present?
 
Some idea of the shaft material would help along with the basic diameter of the shaft you are hardening.
 
What is the size and form of your spline teeth? A spline tooth requiring a 2.5-3mm case depth would likely be extremely large.

Also, I agree with TVP that surface decarb might be an issue.
 