Jan 25, 2006 #1 hector002 Mechanical Joined Jan 11, 2006 Messages 20 Location US what sort of processes would i need to obtain a '12' surface finish on a 4340 steel shaft- can this be obtained just through grinding?
what sort of processes would i need to obtain a '12' surface finish on a 4340 steel shaft- can this be obtained just through grinding?
Jan 25, 2006 1 #2 alexit Mechanical Joined Dec 19, 2003 Messages 348 Location US I assume you mean 12 microinch surface finish, usually grinding will give surface between 4-16 microinch finish. Upvote 0 Downvote
I assume you mean 12 microinch surface finish, usually grinding will give surface between 4-16 microinch finish.
Jan 26, 2006 #3 limct Mechanical Joined Jan 27, 2003 Messages 134 Location HK burnishing would be a good idea too. Best regards, ct Upvote 0 Downvote
Jan 26, 2006 #4 boo1 Mechanical Joined Oct 31, 2001 Messages 2,129 Location US Depends on what is the application the shaft: seals, bearings, diamaeter, coating and enviroment. Plz clarify Upvote 0 Downvote
Depends on what is the application the shaft: seals, bearings, diamaeter, coating and enviroment. Plz clarify