Does anyone know which companies can supply maraging steel 250 and ultra-high strength H13 in wire form with diameter in the reange of 1.4~5mm? I know these two grades normally are avaliable in large bar size.
 
Replies continue below

Recommended for you

Isn't Allvac still making these? The only other choice that comes to mind is Carpenter.
Have you tried any of the specialty medical wire houses (Ft. Wayne?).
All that you may be able to get are straight drawn lengths, not coiled wire. And it will be expensive.....

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps