Good Morning Everyone,
Has anyone had any experience specifying precast concrete foundation walls by Superior Walls?
We have a home builder that brought some details for these things and wants to know if we would allow them as an alternative to poured concrete foundation walls.
These walls have 2"x8" concrete studs at 24" o/c, a 2"x10" top and bottom concrete plate, and the face of the wall is 1 3/4" thick. We are still waiting on answers for reinforcing specs. These wall panels can come in varying lengths and heights. Generally pre-cast stuff is also engineered and approved by the manufacturer however they have made it clear that the liability for these walls to be installed here in Manitoba would be ours.
We understand there is a key provided to lock adjacent panels to each other and then a watersealant/waterstop and waterproofing membrane isapplied.
Anyone have advice or recommendations besides check the wall once we get the rebar specifications?
Has anyone had any experience specifying precast concrete foundation walls by Superior Walls?
We have a home builder that brought some details for these things and wants to know if we would allow them as an alternative to poured concrete foundation walls.
These walls have 2"x8" concrete studs at 24" o/c, a 2"x10" top and bottom concrete plate, and the face of the wall is 1 3/4" thick. We are still waiting on answers for reinforcing specs. These wall panels can come in varying lengths and heights. Generally pre-cast stuff is also engineered and approved by the manufacturer however they have made it clear that the liability for these walls to be installed here in Manitoba would be ours.
We understand there is a key provided to lock adjacent panels to each other and then a watersealant/waterstop and waterproofing membrane isapplied.
Anyone have advice or recommendations besides check the wall once we get the rebar specifications?