I am working on transitioning over to the built-in *Superelastic definitions of nitinol in Abaqus, and at the same time working to include plasticity (new model requires very high strains). I'm having a rough time including the Material Hardening and Material Hardening Modifications.

I built a simple unit-cell mesh and pull on it with various amounts of strain. Here's the output:
Capture_qsqqdq.jpg


There's obviously a few things wrong here, so let's tackle them one at a time (they may actually be linked, but I'll discuss them separately):

Upper plateau stress superelastic window:
The end of my superelastic window should be around 6.5% for this material model. Note, however, when going beyond the martensitic elastic region that with each subsequent loop (12%, 14%, 16%) that the original length of the upper plateau is preserved, so I seemingly have a material which exhibits elasticity almost to 10% after a 15% pull. This is obviously nowhere near correct.

Degradation of plateau stresses with subsequent loops:
I've attempted to use the Super Elastic Hardening Modifications table provided, but the documentation is woefully inadequate (as I've found typical of Abaqus) to actually help a user correctly use the features rather than just tell what is is. I'm wondering if I were able to use this correctly then the length of the upper plateau might also fall in line?

Any thoughts?
 
hard to clarify the issue without the material definition. Can you share that?

If I were you I would try the following:
superelastic material model - apply tension to 6%, unload, reapply tension to 20%. verify output
superelastic plastic material model - apply tension to 6%, unload, reapply tension to 20%, verify output
add plateau stress adjustment - apply tension to 6%, unload, reapply tension to 20%. verify output

there is additional info on the superelastic material models on the Simulia Learning community.
 
Dave-

I've completed those steps, and it all works just fine. The problem arrises, however, when doing the following:

tension to 6%, unload, reapply tension to 12%, unload, reapply tension to 16%, unload, reapply tension to 20%

When tensioning to the 16% and 20% loops, the upper plateau remains as long as it did during the 6% loop, but due to plasticity it started several percent later, thereby making it appear as though the upper plateau can go out to 8, 9, 10% after initial plasticity has begun. Using the hardening suboption I was able to modify this a little, but it isn't great.

With as common as NiTi is used in the med device industry, it baffles me why Simulia hasn't created a better/more friendly method than users writing/using complex user subroutines to adequately capture the stress/strain behavior of the material.
 
why does your stress remain positive. Are you plotting max principal stress?

Plot the directional components of stress/strain. if you loaded the element in the X-direction plot LE11 vs. S11.

if you plot the directional components i think you can see the material model is behaving correctly.
 
ryankb said:
With as common as NiTi is used in the med device industry, it baffles me why Simulia hasn't created a better/more friendly method than users writing/using complex user subroutines to adequately capture the stress/strain behavior of the material.

There is no user friendly method to capture stress/strain behavior of NiTi simply because the material itself isn't user friendly :)

*********************************************************